Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 83 cSt | 83 cSt | Base Oil; ASTM D445 |
Nye Lubricants 402 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 83 cSt | 83 cSt | Base Oil; ASTM D445 |
Nye Lubricants 782KA (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 83 cSt | 83 cSt | Base Oil; ASTM D445 |
Nye Lubricants 782LC (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 83 cSt | 83 cSt | ASTM D445 |
ChevronTexaco Drive Train Fluid HD, SAE 30 FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 .. |
|||
Kinematic Viscosity at 40°C (104°F) | 83 cSt | 83 cSt | |
ChevronTexaco SAE 30 Transmission and Drive Train TO-4 Oil Texaco Transmission and Drive Train TO-4 Oils deliver value through:Longer equipment life — Special additives protect metal surfaces against scuffing and wear even under severe operating conditions.. |