Polymer Property : Kinematic Viscosity at 40°C (104°F) = 83 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 83 cSt
83 cSt
Base Oil; ASTM D445
Nye Lubricants 402 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 83 cSt
83 cSt
Base Oil; ASTM D445
Nye Lubricants 782KA (NG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 83 cSt
83 cSt
Base Oil; ASTM D445
Nye Lubricants 782LC (NG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 83 cSt
83 cSt
ASTM D445
ChevronTexaco Drive Train Fluid HD, SAE 30
FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 ..
Kinematic Viscosity at 40°C (104°F) 83 cSt
83 cSt
ChevronTexaco SAE 30 Transmission and Drive Train TO-4 Oil
Texaco Transmission and Drive Train TO-4 Oils deliver value through:Longer equipment life — Special additives protect metal surfaces against scuffing and wear even under severe operating conditions..