Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil 636 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil 680 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil 680 Mobilgear SHC XMP Series Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin .. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil Extra Hecta Super Mobil Cylinder Oil Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil Mobil Glygoyle 680 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 148 The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil Spartan EP 680 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | |
ConocoPhillips Syncon® EP Gear Oil, AGMA number 8EP Description: Conoco Syncon EMGARD EP Gear Oil 680 is specifically formulated to protect moderate to heavily loaded industrial gears and bearings. It provides excellent antiwear and load-carrying cap.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ChevronTexaco ISO 680 Synthetic Wheel Motor Lubricant EP FeaturesChevron Synthetic Wheel Motor Lubricants EP are superior quality industrial EP gear lubricants. Their advanced formulation provides superior load carrying and antiwear properties; protection.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | See Note 3. |
ChevronTexaco Multifak® HD NLGI Grade 00 Texaco Multifak HD delivers value through:Semi-fluid grease properties provide a thick film of lubricant to critical parts.Low temperature lubrication.Excellent rust and corrosion protectionTacky co.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil 636 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil 680 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil 680 Mobilgear SHC XMP Series Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin .. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil Extra Hecta Super Mobil Cylinder Oil Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil Mobil Glygoyle 680 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 148 The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil Mobilgrease HTS Mobilgrease HTR, HTM, HTS and HTF are high performance Extreme Pressure greases with exceptional resistance to the water contamination conditions typical of steel mill, surface mining, and off-highw.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil Mobilgrease XTC Mobilgrease XTC is an extra high performance product designed for use in high speed coupling applications. It is manufactured with a selected high viscosity mineral base oil and an extremely effecti.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil Spartan EP 680 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | |
ConocoPhillips 680 Gear Oil AGMA Lubricant No. 8EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | |
ConocoPhillips Inca® 680 Oil, AGMA No. 8 Comp. Description: Conoco Inca Oil is a high-quality compounded lubricant recommended for use in heavily loaded industrial and automotive worm gears and bearings operating at moderate to high temperatures.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil Mobilgrease HTS Mobilgrease HTR, HTM, HTS and HTF are high performance Extreme Pressure greases with exceptional resistance to the water contamination conditions typical of steel mill, surface mining, and off-highw.. |
|||
Kinematic Viscosity at 40°C (104°F) | 680 cSt | 680 cSt | ASTM D445 |
ExxonMobil Mobilgrease XTC Mobilgrease XTC is an extra high performance product designed for use in high speed coupling applications. It is manufactured with a selected high viscosity mineral base oil and an extremely effecti.. |