ChevronTexaco Multifak® HD NLGI Grade 00

Category Fluid , Lubricant , Lithium Gellant
Manufacturer ChevronTexaco Corp
Trade Name Multifak® HD
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Multifak® HD NLGI Grade 00.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Multifak HD delivers value through:Semi-fluid grease properties provide a thick film of lubricant to critical parts.Low temperature lubrication.Excellent rust and corrosion protectionTacky consistency reduces the risk of water washout.Texaco Multifak HD is a lithium based semi-fluid grease specially formulated with a high viscosity base oil, and an additive package that contains inhibitors and tackifiers.Texaco Multifak HD is recommended for gear drives that specify an NLGI 00 grease. These include large mowing machines pulled behind tractors and gearboxes in large mixers.Texaco Multifak HD is unsuitable for applications requiring an extreme pressure grease.It is recommended for gear drives specifying a semifluid grease, including those manufactured by:Jacobsen Division of TextronNORD Gear CorporationTypical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication. Determined on mineral oil extracted by vacuum filtration.Unknown amount of work.CPS Number: 221988; MSDS Number: 9006
Physical Properties Metric English Comments
Viscosity Measurement 78
78
Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 3709 SUS
3709 SUS
See Note 3.
Saybolt Viscosity at 210°F 167 SUS
167 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 680 cSt
680 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 34 cSt
34 cSt
See Note 3.
Mechanical Properties Metric English Comments
Penetration 4.0
4.0
% Change, (10000X), 25°C, See Note 5.
Penetration P(60), 1/10 mm 415
415
Unknown Amount of Work, 25°C (77°F)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
See Note 2.
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
See Note 1.
Dropping Point 166 °C
331 °F
Descriptive Properties Value Comments
Color Brown
Rust Prevention Pass
Texture Tacky
Thickener, % 1.9
Lithium