Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 670 cSt
670 cSt
ASTM D445
ExxonMobil 680 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
Kinematic Viscosity at 40°C (104°F) 670 cSt
670 cSt
ASTM D445
ExxonMobil 680 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
Kinematic Viscosity at 40°C (104°F) 670 cSt
670 cSt
ConocoPhillips 680 Bearing Oil
Description: Conoco Bearing Oil is formulated for the circulating systems that lubricate roll-neck bearings in steel and nonferrous rolling mills. It is suited for systems in which water and corrosi..