Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 670 cSt | 670 cSt | ASTM D445 |
ExxonMobil 680 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Kinematic Viscosity at 40°C (104°F) | 670 cSt | 670 cSt | ASTM D445 |
ExxonMobil 680 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Kinematic Viscosity at 40°C (104°F) | 670 cSt | 670 cSt | |
ConocoPhillips 680 Bearing Oil Description: Conoco Bearing Oil is formulated for the circulating systems that lubricate roll-neck bearings in steel and nonferrous rolling mills. It is suited for systems in which water and corrosi.. |