Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 440 cSt | 440 cSt | Base Oil; ASTM D445 |
Nye Lubricants 794 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 440 cSt | 440 cSt | Base Oil; ASTM D445 |
Nye Lubricants 794RP (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 440 cSt | 440 cSt | |
ConocoPhillips IGL-9 Enclosed Gear Lubricant ISO 460, AGMA Number 7EP Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service co.. |