Nye Lubricants 794 (RL) Synthetic Oil

Category Fluid , Lubricant , Clay Gellant , Synthetic Ether Base
Manufacturer Nye Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 794 (RL) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 107
107
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 440 cSt
440 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 32.4 cSt
32.4 cSt
Base Oil; ASTM D445
Evaporation Loss 0.80 %
0.80 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 253
253
ASTM D217
Penetration P(60), 1/10 mm 276
276
ASTM D217
Oil Separation 1.2 %
1.2 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Recommended
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Recommended
Pour Point -25.0 °C
-13.0 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type Ester(Blnd)
Gellant Type Clay