Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 42 cSt | 42 cSt | Base Oil; ASTM D445 |
Nye Lubricants 363AX-1 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 42 cSt | 42 cSt | ASTM D445 |
ExxonMobil 10W Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |
|||
Kinematic Viscosity at 40°C (104°F) | 42 cSt | 42 cSt | ASTM D445 |
ExxonMobil 10W Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |
|||
Kinematic Viscosity at 40°C (104°F) | 42 - 50 cSt | 42 - 50 cSt | |
ELM® SoyFluid™ Hydraulic Universal Tractor Biodegradable Tractor Hydraulic-Transmission Fluid Description: ELM SoyFluid™ Hydraulic Universal Tractor is a readily biodegradable tractor hydraulic transmission fluid formulated with Biotechbased™ USA grown natural vegetable oils. This product.. |
|||
Kinematic Viscosity at 40°C (104°F) | 42 cSt | 42 cSt | |
ConocoPhillips 46 FC Fluid-D ISO Description: Conoco FC Fluid-D is a premixed, ready-to-use fluid for hydraulic systems, such as those found in underground-mining equipment that operate where fire-hazard and other personnel safety .. |