ELM® SoyFluid™ Hydraulic Universal Tractor Biodegradable Tractor Hydraulic-Transmission Fluid

Category Fluid , Lubricant
Manufacturer ELM®
Trade Name SoyFluid™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELM® SoyFluid™ Hydraulic Universal Tractor Biodegradable Tractor Hydraulic-Transmission Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ELM SoyFluid™ Hydraulic Universal Tractor is a readily biodegradable tractor hydraulic transmission fluid formulated with Biotechbased™ USA grown natural vegetable oils. This product surpasses the performance and lubricity of most conventional oils.Applications: Designed for equipment using a shared hydraulic fluid reservoir operating clutches, brakes and lift systemsBenefits: Protects against wear, brake chatter and clutch slippageSuperior lubricity protects pumps, valves, cylinders and other hydraulic componentsPrevents corrosion of non-ferrous metal partsIs compatible with most hydraulic hoses and sealsVirtually biodegradable formulation provides the most safety for the environmentMeets USDA proposed definition EO 13101 for Biobased productsManufactured in USA from USA grown crop-based oilsInformation provided by ELM®
Physical Properties Metric English Comments
Viscosity Measurement 230
230
Index
Kinematic Viscosity at 40°C (104°F) 42 - 50 cSt
42 - 50 cSt
Thermal Properties Metric English Comments
Pour Point -25.0 °C
-13.0 °F
Flash Point 256 °C
493 °F
Descriptive Properties Value Comments
Rust & Corrosion 1A
ASTM D130