Polymer Property : Kinematic Viscosity at 40°C (104°F) = 41 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 41 cSt
41 cSt
ASTM D445
ChevronTexaco Bright-Cut® AH Metal Working Fluid
FeaturesChevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.The unique synthetic antiweld components ..
Kinematic Viscosity at 40°C (104°F) 41 cSt
41 cSt
ChevronTexaco Hydraulic Safety Fluid
Texaco Hydraulic Safety Fluid is a fire-resistant fluid designed for use in high pressure hydraulic systems where the requirements for fire resistance, pump wear protection and viscosity are satisfi..