Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 34.3 cSt | 34.3 cSt | |
ConocoPhillips Synterra™ 32 Hydraulic Oil 32 Conoco Synterra Environmental Fluids Hydraulic and Circulating Oils give outstanding protection to equipment and the environment. These oils are made from synthetic polyol ester fluids and come in f.. |