Polymer Property : Kinematic Viscosity at 40°C (104°F) = 34.3 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 34.3 cSt
34.3 cSt
ConocoPhillips Synterra™ 32 Hydraulic Oil 32
Conoco Synterra Environmental Fluids Hydraulic and Circulating Oils give outstanding protection to equipment and the environment. These oils are made from synthetic polyol ester fluids and come in f..