Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 235 cSt
235 cSt
ASTM D445
ExxonMobil Mobil Polyrex EP 2
Mobil Polyrex EP 2 is a shear-stable polyurea grease with excellent extreme-pressure (EP) and load-carrying characteristics. The proprietary polyurea thickener system exhibits excellent resistance t..
Kinematic Viscosity at 40°C (104°F) 235 cSt
235 cSt
Base Oil
ConocoPhillips Syncon® EP Heavy Duty Grease NLGI 1
Description: Conoco Syncon EP Heavy Duty Grease is an ultra high-performance synthetic base oil, lithium-complex grease specifically designed for extreme loading conditions. The combination of high-..
Kinematic Viscosity at 40°C (104°F) 235 cSt
235 cSt
Base Oil
ConocoPhillips Syncon® EP Heavy Duty Grease NLGI 2
Description: Conoco Syncon EP Heavy Duty Grease is an ultra high-performance synthetic base oil, lithium-complex grease specifically designed for extreme loading conditions. The combination of high-..
Kinematic Viscosity at 40°C (104°F) 235 cSt
235 cSt
Base Oil
ConocoPhillips Tacna® EP Polyurea Grease NLGI Grade 1
Description: Conoco Tacna EP Polyurea Grease is a shear-stable product with exceptional extreme-pressure characteristics and excellent water resistance. It is recommended for use in steel mills, off..
Kinematic Viscosity at 40°C (104°F) 235 cSt
235 cSt
Base Oil
ConocoPhillips Tacna® EP Polyurea Grease NLGI Grade 2
Description: Conoco Tacna EP Polyurea Grease is a shear-stable product with exceptional extreme-pressure characteristics and excellent water resistance. It is recommended for use in steel mills, off..
Kinematic Viscosity at 40°C (104°F) 235 cSt
235 cSt
ASTM D445
ExxonMobil Mobil Polyrex EP 2
Mobil Polyrex EP 2 is a shear-stable polyurea grease with excellent extreme-pressure (EP) and load-carrying characteristics. The proprietary polyurea thickener system exhibits excellent resistance t..