Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 235 cSt | 235 cSt | ASTM D445 |
ExxonMobil Mobil Polyrex EP 2 Mobil Polyrex EP 2 is a shear-stable polyurea grease with excellent extreme-pressure (EP) and load-carrying characteristics. The proprietary polyurea thickener system exhibits excellent resistance t.. |
|||
Kinematic Viscosity at 40°C (104°F) | 235 cSt | 235 cSt | Base Oil |
ConocoPhillips Syncon® EP Heavy Duty Grease NLGI 1 Description: Conoco Syncon EP Heavy Duty Grease is an ultra high-performance synthetic base oil, lithium-complex grease specifically designed for extreme loading conditions. The combination of high-.. |
|||
Kinematic Viscosity at 40°C (104°F) | 235 cSt | 235 cSt | Base Oil |
ConocoPhillips Syncon® EP Heavy Duty Grease NLGI 2 Description: Conoco Syncon EP Heavy Duty Grease is an ultra high-performance synthetic base oil, lithium-complex grease specifically designed for extreme loading conditions. The combination of high-.. |
|||
Kinematic Viscosity at 40°C (104°F) | 235 cSt | 235 cSt | Base Oil |
ConocoPhillips Tacna® EP Polyurea Grease NLGI Grade 1 Description: Conoco Tacna EP Polyurea Grease is a shear-stable product with exceptional extreme-pressure characteristics and excellent water resistance. It is recommended for use in steel mills, off.. |
|||
Kinematic Viscosity at 40°C (104°F) | 235 cSt | 235 cSt | Base Oil |
ConocoPhillips Tacna® EP Polyurea Grease NLGI Grade 2 Description: Conoco Tacna EP Polyurea Grease is a shear-stable product with exceptional extreme-pressure characteristics and excellent water resistance. It is recommended for use in steel mills, off.. |
|||
Kinematic Viscosity at 40°C (104°F) | 235 cSt | 235 cSt | ASTM D445 |
ExxonMobil Mobil Polyrex EP 2 Mobil Polyrex EP 2 is a shear-stable polyurea grease with excellent extreme-pressure (EP) and load-carrying characteristics. The proprietary polyurea thickener system exhibits excellent resistance t.. |