Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 215 cSt | 215 cSt | Base Oil; ASTM D445 |
Nye Lubricants 367MS (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 215 cSt | 215 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 1419 Mobil Vacuoline 1400 Series oils are extra high performance lubricants specifically designed to satisfy the requirements of machine tools that use one oil for both hydraulic systems and way lubricat.. |
|||
Kinematic Viscosity at 40°C (104°F) | 215 cSt | 215 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 1419 Mobil Vacuoline 1400 Series oils are extra high performance lubricants specifically designed to satisfy the requirements of machine tools that use one oil for both hydraulic systems and way lubricat.. |
|||
Kinematic Viscosity at 40°C (104°F) | 215 cSt | 215 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® 6220 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |