Polymer Property : Kinematic Viscosity at 40°C (104°F) = 215 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 215 cSt
215 cSt
Base Oil; ASTM D445
Nye Lubricants 367MS (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 215 cSt
215 cSt
ASTM D445
ExxonMobil Mobil Vaculine 1419
Mobil Vacuoline 1400 Series oils are extra high performance lubricants specifically designed to satisfy the requirements of machine tools that use one oil for both hydraulic systems and way lubricat..
Kinematic Viscosity at 40°C (104°F) 215 cSt
215 cSt
ASTM D445
ExxonMobil Mobil Vaculine 1419
Mobil Vacuoline 1400 Series oils are extra high performance lubricants specifically designed to satisfy the requirements of machine tools that use one oil for both hydraulic systems and way lubricat..
Kinematic Viscosity at 40°C (104°F) 215 cSt
215 cSt
ASTM D-445
ConocoPhillips ANDEROL® 6220 Synthetic Food Grade Gear Fluid
Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the ..