Polymer Property : Kinematic Viscosity at 40°C (104°F) = 18 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 18 cSt
18 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8951 (897-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 18 cSt
18 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8951R (897RP-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.