Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 18 cSt | 18 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8951 (897-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 18 cSt | 18 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8951R (897RP-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 18 cSt | 18 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8955 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 18 cSt | 18 cSt | Base Oil; ASTM D445 |
Nye Lubricants 799 (RL) Synthetic Oil Information provided by Nye Lubricants. |