Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Kinematic Viscosity at 40°C (104°F) = 14 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 14 cSt
14 cSt
Base Oil; ASTM D445
Nye Lubricants 200 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 14 cSt
14 cSt
Base Oil; ASTM D445
Nye Lubricants 203 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 14 cSt
14 cSt
Base Oil; ASTM D445
Nye Lubricants 200RP (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 14 cSt
14 cSt
ASTM D445
ExxonMobil Exterex™ A41 Synthetic Fluid
Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol..
Copyright © lookpolymers.com All Rights Reserved