Material Notes:
Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low volatilities. Esterex™ Adipate Esters can be used as sole basestocks or blendstocks with other synthetic fluids in many automotive and industrial lubricant applications. These esters are ideal in high-temperature conditions, such as reciprocating air compressors, where discharge valve cleanliness is required. Appearance: Bright & ClearAvailability: Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.921 g/cc

@Temperature 15.6 °C
0.0333 lb/in³

@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 144
144
Index; ASTM D2270
Kinematic Viscosity 3286 cSt

@Temperature -40.0 °C
3286 cSt

@Temperature -40.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 14 cSt
14 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 3.6 cSt
3.6 cSt
ASTM D445
Evaporation Loss 22.3 %

@Temperature 205 °C,
Time 23400 sec
22.3 %

@Temperature 401 °F,
Time 6.50 hour
ASTM D972
Thermal Properties Metric English Comments
Pour Point -57.2 °C
-71.0 °F
ASTM D5950/D97
Flash Point 231 °C
448 °F
COC; ASTM D92
249 °C
480 °F
PMCC; ASTM D92
Optical Properties Metric English Comments
Refractive Index 1.4505
1.4505
ASTM D1218
Chemical Properties Metric English Comments
Acid Value 0.010
0.010
[mg KOH/g]; ASTM D974 (mod)
Descriptive Properties Value Comments
Aniline Point <68°F
ASTM D611
Biodegradation 0.765
OECD 301F
Color <0.5
ASTM D1500
Composition Water
<500 ppm, ASTM D6304 (mod)
Density Correction Factor 0.000718 (g/cc)/°C
ASTM D1250
Elastomer Compatibility -0.04
Fluoroelastomer Hardness Change, ASTM D471
-0.066
Fluoroelastomer Tensile Strength Change, ASTM D471
0.083
Fluoroelastomer Volume Change, ASTM D471
-0.091
Fluoroelastomer Elongation Change, ASTM D471
-0.12
Nitrile Hardness Change, ASTM D471
-0.17
Polyacrylate Hardness Change, ASTM D471
-0.22
Polyacrylate Elongation Change, ASTM D471
0.235
Nitrile Volume Change, ASTM D471
-0.383
Polyacrylate Tensile Strength Change, ASTM D471
-0.413
Nitrile Elongation Change, ASTM D471
0.427
Polyacrylate Volume Change, ASTM D471
-0.505
Nitrile Tensile Strength Change, ASTM D471
Fire point 480°F
COC, ASTM D92
Hydrolytic Stability, TAN Change 0.13 mg KOH/g
ASTM D2619
Kauri-Butanol Value 72
ASTM D1133
Noack Volatility 0.156
ASTM D5800/DIN 51581
RPVOT >1210 min
With AO, ASTM D2272
415 min
Neat, ASTM D2272