Polymer Property : Kinematic Viscosity at 40°C (104°F) = 13 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 13 cSt
13 cSt
ASTM D445
ExxonMobil Mobilarma 777
The Mobilarma 700 Series contains three premium performance rust preventives that cover a range of applications including storage and inter-operational activities. The Mobilarma 777 and 778 are inte..
Kinematic Viscosity at 40°C (104°F) 13 cSt
13 cSt
ASTM D445
ChevronTexaco Superla® DCO
FeaturesChevron Superla DCO is a highly refined food grade white mineral oil that exceeds FDA purity requirements for the dedusting of grains intended for human consumption.Chevron Superla DCO conta..
Kinematic Viscosity at 40°C (104°F) 13 cSt
13 cSt
ChevronTexaco Transultex® CF A
Texaco Transultex CF metalworking fluids deliver value through:Excellent antiweld properties from active sulfur and chlorine-free EP compounding which reduce frictional heat, prevent welding of meta..
Kinematic Viscosity at 40°C (104°F) 13 cSt
13 cSt
ASTM D445
ExxonMobil Mobilarma 777
The Mobilarma 700 Series contains three premium performance rust preventives that cover a range of applications including storage and inter-operational activities. The Mobilarma 777 and 778 are inte..
Kinematic Viscosity at 40°C (104°F) 13 cSt
13 cSt
ChevronTexaco Alcaid® 13
Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition..