ChevronTexaco Superla® DCO

Category Fluid , Lubricant , White Mineral Oil (WMO)
Manufacturer ChevronTexaco Corp
Trade Name Superla®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Superla® DCO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron Superla DCO is a highly refined food grade white mineral oil that exceeds FDA purity requirements for the dedusting of grains intended for human consumption.Chevron Superla DCO contains vitamin E, a natural antioxidant, to protect quality during handling and storage.ApplicationsChevron Superla DCO can be used to control dust on animal feeds, chemicals, and fertilizers.Food grade white mineral oils are widely used for dust control by the grain industry. White oil is applied to the grain just before or during active grain tumbling to prevent dust from escaping the grain stream. For best results, the oil should be applied before the grain enters the storage bin. Only food grade oils that meet the tough standards of the U.S. Food and Drug Administration (FDA) may be used for this application. Chevron Superla DCO does not promote grain rancidity.Chevron Superla DCO is a field-proven products, fully authorized by the FDA for grain dedusting – at concentrations up to 200 ppm on the grain or rice.
Physical Properties Metric English Comments
API Gravity 34.8 °
34.8 °
Saybolt Viscosity at 100°F 74 SUS
74 SUS
Kinematic Viscosity at 40°C (104°F) 13 cSt
13 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -12.0 °C
10.4 °F
ASTM D97
Flash Point 177 °C
351 °F
ASTM D92
Descriptive Properties Value Comments
Color +30 Saybolt