Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 111 cSt | 111 cSt | Base Oil; ASTM D445 |
Nye Lubricants 365 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 111 cSt | 111 cSt | Base Oil; ASTM D445 |
Nye Lubricants 365A-MS (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 111 cSt | 111 cSt | Base Oil; ASTM D445 |
Nye Lubricants 365F (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 111 cSt | 111 cSt | Base Oil; ASTM D445 |
Nye Lubricants 365FT (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 111 cSt | 111 cSt | |
ChevronTexaco Texglass MV Texaco Texglass MV delivers value through:Ability to maintain film thickness — High viscosity index indicates an oil that maintains film thickness at high temperatures.Sludge protection — Detergen.. |
|||
Kinematic Viscosity at 40°C (104°F) | 111 cSt | 111 cSt | ASTM D445 |
ExxonMobil SAE 30 Mobilgard 300 Mobilgard 300 by ExxonMobil is a premium quality, extra high performance system oil designed for crosshead diesel engines. High quality paraffinic base oils along with a balanced additive system pro.. |
|||
Kinematic Viscosity at 40°C (104°F) | 111 cSt | 111 cSt | ASTM D445 |