ChevronTexaco Texglass MV

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Texglass
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Texglass MV.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Texglass MV delivers value through:Ability to maintain film thickness — High viscosity index indicates an oil that maintains film thickness at high temperatures.Sludge protection — Detergents and dispersants minimize deposits on metal surfaces.Rust protection — Contains a rust inhibitor to protect metal surfaces.Long lubricant life — Resists thermal oxidation and viscosity increase, providing long lubricant life.Foam inhibitionTexaco Texglass MV is a machine oil designed for use in the glass manufacturing process.It is manufactured from highly refined mineral base oils and contains an additive package with antiwear, dispersant and detergent properties.It has a high viscosity index to assure good film strength between metal surfaces under moderate loads and temperatures. This film strength is further enhanced by the antiwear additive protection.The foam and aeration suppressant allows the quick release of entrained air, also improving film strength.Texaco Texglass MV is recommended as a machine oil and constant cushion oil for I.S. glass machines. It is also designed for use in linkage and gearboxes, central lubrication systems, mechanical gob distributors, blowhead and funnel cams.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 222628; MSDS Number: 8911
Physical Properties Metric English Comments
API Gravity 29.8 °
29.8 °
Viscosity Measurement 134
134
Viscosity Index
Saybolt Viscosity at 100°F 572 SUS
572 SUS
Saybolt Viscosity at 210°F 77.5 SUS
77.5 SUS
Kinematic Viscosity at 40°C (104°F) 111 cSt
111 cSt
Kinematic Viscosity at 100°C (212°F) 14.5 cSt
14.5 cSt
Thermal Properties Metric English Comments
Pour Point -38.0 °C
-36.4 °F
Flash Point 234 °C
453 °F
Descriptive Properties Value Comments
Foaming Tendency, mL 15
Sequence II, 0 min