Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 626 cSt | 626 cSt | |
Lubriplate 1444 Aluminum Complex Multi-Purpose Grease Tacky aluminum complex grease specifically formulated for heavy-duty construction and mining equipment. Excellent for slow to moderate speed bearings and chains that are subjected to heat, steam, an.. |