Lubriplate 1444 Aluminum Complex Multi-Purpose Grease

Category Fluid , Lubricant , Aluminum Gellant
Manufacturer Lubriplate Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate 1444 Aluminum Complex Multi-Purpose Grease.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tacky aluminum complex grease specifically formulated for heavy-duty construction and mining equipment. Excellent for slow to moderate speed bearings and chains that are subjected to heat, steam, and water.Applications: Heavy-duty construction, mining equip. 1444 is available in Cartridges, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 3300 SUS
3300 SUS
Kinematic Viscosity at 40°C (104°F) 626 cSt
626 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 265
265
Unknown Amount of Work
Penetration P(60), 1/10 mm 295
295
Unknown Amount of Work
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -12.2 °C
10.0 °F
Approx. Cold test
Dropping Point 260 °C
500 °F
ASTM Test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW/EP
NLGI Grade 2
Rust/Oxidative Additives YES
Water Resistant YES