Polymer Property : Kinematic Viscosity at 40°C (104°F) = 47 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 47 cSt
47 cSt
Lubriplate SYNCOOL 46 Polyglycolester-Based Synthetic Air Compressor Fluid
These polyglycolester-based synthetic fluids are designed for rotary screw air compressors. They offer excellent heat transfer properties, low evaporation, high flash points, and outstanding oxidati..