Material Notes:
These polyglycolester-based synthetic fluids are designed for rotary screw air compressors. They offer excellent heat transfer properties, low evaporation, high flash points, and outstanding oxidation resistance, eliminating varnish and sludge. Fluid change intervals are 8,000 hours under normal operating conditions. Syncool Series Fluids are available in Pails & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 46
46
ISO Grade
180
180
Viscosity Index
Saybolt Viscosity at 100°F 232 SUS
232 SUS
Saybolt Viscosity at 210°F 55 SUS
55 SUS
Kinematic Viscosity at 40°C (104°F) 47 cSt
47 cSt
Kinematic Viscosity at 100°C (212°F) 9.0 cSt
9.0 cSt
Thermal Properties Metric English Comments
Pour Point -45.6 °C
-50.0 °F
Flammability Test 555
555
[°F] Fire Point
Flash Point 243 °C
470 °F
Descriptive Properties Value Comments
SAE No. 20