Polymer Property : Kinematic Viscosity at 40°C (104°F) = 355 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 355 cSt
355 cSt
ASTM D445
Solvay Specialty Polymers FOMBLIN® Z60 PFPE Lubricant
FOMBLIN® Z is a linear PFPE available as a neutral or functionalized fluid. They are used in aerospace, magnetic media, and polymer modification uses.Information provided by Solvay Solexis, Inc...