Solvay Specialty Polymers FOMBLIN® Z60 PFPE Lubricant

Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name FOMBLIN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers FOMBLIN® Z60 PFPE Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FOMBLIN® Z is a linear PFPE available as a neutral or functionalized fluid. They are used in aerospace, magnetic media, and polymer modification uses.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ASTM D891
Viscosity Measurement 360
360
Viscosity Index; ASTM D2270
Kinematic Viscosity 600 cSt

@Temperature 20.0 °C
600 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 355 cSt
355 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 98 cSt
98 cSt
ASTM D445
Molecular Weight 13000 g/mol
13000 g/mol
Evaporation Loss 0.20 %
0.20 %
22 hrs. at 204°C; ASTM 2595
Surface Tension 25 dynes/cm
25 dynes/cm
ASTM D1331
Thermal Properties Metric English Comments
Pour Point -63.0 °C
-81.4 °F
ASTM D97