Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 125 SUS
125 SUS
Heatbath/Park Vacuum Quench Oil
For use in quenching in integral vacuum furnaces. Offers excellent quenching rate and thermal stability, good viscosity, and low volatility.Information provided by Heatbath Corporation - Park Metal..