Physical Properties Metric English Comments
Filament Diameter 6.9 µm
6.9 µm
Hexcel® HexTow™ AS4C Carbon Fiber
HexTow™ AS4C carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. This fiber has been surface treated..
Filament Diameter 6.9 µm
6.9 µm
Hexcel® HexTow™ AS7 Carbon Fiber
HexTow™ AS7 carbon fiber is a continuous, high strength, high strain, PAN based fiber available, in a 12,000 (12K) filament count tow. This fiber has been surface treated and can be sized to improv..
Filament Diameter 6.9 µm
6.9 µm
Hexcel® HexTow™ AS2C Carbon Fiber
HexTow™ AS2C carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. This fiber has been surface treated..