Physical Properties | Metric | English | Comments |
---|---|---|---|
Filament Diameter | 5.0 - 25 µm | 5.0 - 25 µm | |
AGY ZenTron® S-2 Generic S-Glass Fiber S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Mod.. |