Physical Properties | Metric | English | Comments |
---|---|---|---|
Filament Diameter | 180 - 350 µm | 180 - 350 µm | |
EMS-Griltech Grilamid® DN 10 Nylon 12 Monofilament Description: GRILAMID Monofilaments are mainly used in Filtration. Data provided by Description: GRILAMID Monofilaments are mainly used in Filtration. Data provided by EMS-Griltech. |
|||
Filament Diameter | 180 - 1000 µm | 180 - 1000 µm | |
EMS-Griltech Grilon® BM 10 Nylon 6 Monofilament (Medium-Set) Description: GRILON BM 10 is a Nylon 6 based monofilament for filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech. |
|||
Filament Diameter | 180 - 260 µm | 180 - 260 µm | |
EMS-Griltech Grilon® BN 19 Nylon 6 Monofilament (Non-Set) Description: GRILON BN 19 is a Nylon 6 based monofilament for filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech. |