Physical Properties Metric English Comments
Filament Diameter 180 - 350 µm
180 - 350 µm
EMS-Griltech Grilamid® DN 10 Nylon 12 Monofilament
Description: GRILAMID Monofilaments are mainly used in Filtration. Data provided by Description: GRILAMID Monofilaments are mainly used in Filtration. Data provided by EMS-Griltech.
Filament Diameter 180 - 1000 µm
180 - 1000 µm
EMS-Griltech Grilon® BM 10 Nylon 6 Monofilament (Medium-Set)
Description: GRILON BM 10 is a Nylon 6 based monofilament for filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech.
Filament Diameter 180 - 260 µm
180 - 260 µm
EMS-Griltech Grilon® BN 19 Nylon 6 Monofilament (Non-Set)
Description: GRILON BN 19 is a Nylon 6 based monofilament for filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech.