Physical Properties | Metric | English | Comments |
---|---|---|---|
Filament Diameter | 13 µm | 13 µm | |
SGL Carbon Group PANOX® FA C063 EEA High performance Crimped staple oxidized textile fiber, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Filament Diameter | 13 µm | 13 µm | |
SGL Carbon Group PANOX® FA C063 SSC High performance Crimped staple oxidized textile fiber, For felts and non-wovens PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Filament Diameter | 13 µm | 13 µm | |
SGL Carbon Group PANOX® FA T320 EEA High performance oxidized textile fiber, Continuous Tow with 320k filaments For carbon/carbon and spinning. PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not b.. |
|||
Filament Diameter | 13 µm | 13 µm | |
SGL Carbon Group PANOX® FB M400 EEA Oxidized Textile Fiber, Milled Fiber, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Filament Diameter | 13 µm | 13 µm | |
SGL Carbon Group PANOX® FB T320 EEA Oxidized Textile Fiber, Continuous Tow with 320k filaments, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Filament Diameter | 13 µm | 13 µm | |
SGL Carbon Group PANOX® FM C063 EEA Oxidized Textile Fiber, Crimped staple fiber, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Filament Diameter | 13 µm | 13 µm | |
SGL Carbon Group PANOX® FM C063 SSC Oxidized Textile Fiber, Crimped staple fiber, For felts and non-wovens PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Filament Diameter | 13 µm | 13 µm | |
SGL Carbon Group PANOX® FM T320 EEA Oxidized Textile Fiber, Continuous Tow with 320k filaments, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |