Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.85 g/cc | 7.85 g/cc | |
Carpenter Vega® Alloy Tool Steel (Air-Tough) (AISI A6) Vega die steel combines the deep hardening and minimum size change characteristics of air-hardening steels with the simplicity of low temperature heat treatment possible in many oil-hardening steels.. |