Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.84 g/cc | 7.84 g/cc | |
Latrobe CM-50â„¢ ASTM M50 High Speed Steel CM-50 is classified as an intermediate type high speed steel of the molybdenum chromium- vanadium variety. It is recommended for applications with moderate cutting conditions, such as woodworking to.. |