Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 7.40 g/cc | 7.40 g/cc | |
Nihon Superior SN100C Lead-Free Solder Alloy Allows high productivity in soldering processes and cost effective, reliable joints. Attributes include high fluidity, low copper erosion, low drossing, superior wetting and freedom from shrinkage d.. |