Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 5.85 g/cc | 5.85 g/cc | |
Aremco AREMCOLOX™ 502-1900-MTTZ Dense MgO Partially Stabilized Zirconium Oxide This grade offers a high level of fracture toughness for a zirconia material. Features include excellent fracture, corrosion, thermal shock, and wear resistance. Used for pump parts, valve component.. |
|||
Specific Gravity | 5.85 g/cc | 5.85 g/cc | |
Aremco AREMCOLOX™ 502-1900-YTZP Dense Yttria Stabilized Zirconium Oxide This grade offers a high flexural strength for a zirconia. The fine grain size lends itself to be used in cutting tools where a very sharp edge can be achieved and maintained due to its high wear re.. |