Polymer Property : Specific Gravity = 4.49 g/cc
Polymer Property :
Specific Gravity =
4.49 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Specific Gravity
4.49
g/cc
4.49
g/cc
ASTM D792
PolyOne Gravi-Tech™ GRV-UR-045-SS-W Black Polyurethane, Unspecified (PUR, Unspecified)
Information provided by PolyOne