Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.40 - 3.60 g/cc | 3.40 - 3.60 g/cc | ASTM D792 |
P & P Technology EC-H Silver Copper Loaded Silicone P & P Technology material reference EC-H is a printing grade silicone elastomer with a Silver/Copper conductive filler and is Tan in color. The material is specially compounded to offer excellent p.. |
|||
Specific Gravity | 3.00 - 3.60 g/cc | 3.00 - 3.60 g/cc | |
Parker Chomerics CHO-BOND SV712 Conductive Epoxy CHO-BOND® 700 Series Adhesives for Microelectronics Packaging; these pure silver-filled epoxy pastes are designed to meet the demanding requirements of semiconductor and microelectronic packaging. .. |