Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 3.30 g/cc
3.30 g/cc
ASTM D792
Parker Chomerics CHO-FORM® 5518 Robotically Dispensed Gasketing
Description: CHO-FORM® 5518 Two-component, thermal cure silicone system with Ag/Cu particle filler. Minimum cure temperature is only 85°C (185°F). Formulated for painted, plated or metalized plas..
Specific Gravity 3.30 g/cc
3.30 g/cc
JIS-K-6220; ASTM D-792
Fujipoly Industries Sarcon® XR-e Gap Filler Pad
Sarcon XR-e and XR-j are highly conformable/thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of compon..
Specific Gravity 3.30 - 3.35 g/cc
3.30 - 3.35 g/cc
ASTM D792
Adamas Adalon® 826 PTFE, 50% Stainless steel
Information provided by Adamas, HPM