Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.23 - 2.99 g/cc | 2.23 - 2.99 g/cc | |
Parker Chomerics Tecknit Teckfip™ HC FIP-C Formed in Place Conductive Elastomer Description: Heat cure compound. This compound is an all round high performance compound, and is very similar to a Consil C molded or extruded elastomer. It has been traditionally used for telecommu.. |