Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.77 g/cc | 2.77 g/cc | ASTM D792 |
Rogers Corporation TMM® TMM10 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Specific Gravity | 2.77 g/cc | 2.77 g/cc | ASTM D792 |
Rogers Corporation TMM® TMM101 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |