Polymer Property : Specific Gravity = 2.77 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.77 g/cc
2.77 g/cc
ASTM D792
Rogers Corporation TMM® TMM10 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
Specific Gravity 2.77 g/cc
2.77 g/cc
ASTM D792
Rogers Corporation TMM® TMM101 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..