Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.61 - 2.11 g/cc | 1.61 - 2.11 g/cc | ASTM D792 |
Parker Chomerics Tecknit Consil®-E 811 Extruded Silver-Filled Silicone Elastomer Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se.. |
|||
Specific Gravity | 1.61 - 2.11 g/cc | 1.61 - 2.11 g/cc | ASTM D792 |
Parker Chomerics Tecknit Consil®-II 842 Molded Silver-Filled Silicone Elastomer Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi.. |