Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.91 - 2.01 g/cc | 1.91 - 2.01 g/cc | NBR NM-IEC 60811-1-3 |
Karina White Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.95 - 2.01 g/cc | 1.95 - 2.01 g/cc | ASTM D 792 |
Karina 10/70-IE White Color Concentrate MBU EVA based color concentrate, with 70% of titanium dioxide, recommended for application in polyolefinic and PVC compounds for general purposes. Minimum recommended usage of 0.5%.Information provided.. |
|||
Specific Gravity | 1.95 - 2.01 g/cc | 1.95 - 2.01 g/cc | |
Bulk Molding Compounds BMC 1603 Multi-purpose grade BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 160.. |
|||
Specific Gravity | 1.95 - 2.01 g/cc | 1.95 - 2.01 g/cc | |
Bulk Molding Compounds BMC SLC 1000 Glass Reinforced Polyester BMC SLC 1000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. It is V-0 flame arc and track resistant. UL® recognized. This material was formerly known.. |