Polymer Property : Specific Gravity = 1.98 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.93 - 1.98 g/cc
1.93 - 1.98 g/cc
ISO 1183
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very ..
Specific Gravity 1.90 - 1.98 g/cc
1.90 - 1.98 g/cc
ASTM D792
Adamas Adalon® 403 PTFE, 15% Polyimide
Information provided by Adamas, HPM
Specific Gravity 1.94 - 1.98 g/cc
1.94 - 1.98 g/cc
ASTM D792
Adamas Adalon® 436 PTFE, 15% Ekonol®
Information provided by Adamas, HPM